Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 20.0 °C | 520 MPa Show Material materials with Streckgrenze of 520 MPa | |
540.0 °C | 110 MPa Show Material materials with Streckgrenze of 110 MPa | ||
650.0 °C | 57 MPa Show Material materials with Streckgrenze of 57 MPa | ||
Zugfestigkeit | 20.0 °C | 790 MPa Show Material materials with Zugfestigkeit of 790 MPa | |
540.0 °C | 140 MPa Show Material materials with Zugfestigkeit of 140 MPa | ||
650.0 °C | 86 MPa Show Material materials with Zugfestigkeit of 86 MPa | ||
Chemical properties
Property | Value |
---|---|
Chrom | 0.65 % Show Material materials with Chrom of 0.65 % |
Eisen | 96.6 - 100 % Show Material materials with Eisen of 96.6 - 100 % |
Kohlenstoff | 0.4 % Show Material materials with Kohlenstoff of 0.4 % |
Mangan | 0.8 % Show Material materials with Mangan of 0.8 % |
Nickel | 1.25 % Show Material materials with Nickel of 1.25 % |
Silizium | 0.3 % Show Material materials with Silizium of 0.3 % |