Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.6 - 7.7 g/cm³ Show Material materials with Dichte of 7.6 - 7.7 g/cm³ | Typical for Martensitic Stainless Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 220 GPa Show Material materials with Elastizitätsmodul of 220 GPa | Typical for Martensitic Stainless Steel |
Flächenreduzierung | 20.0 °C | 53 % Show Material materials with Flächenreduzierung of 53 % | |
540.0 °C | 44 % Show Material materials with Flächenreduzierung of 44 % | ||
650.0 °C | 97 % Show Material materials with Flächenreduzierung of 97 % | ||
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Martensitic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Martensitic Stainless Steel |
Streckgrenze | 20.0 °C | 690 MPa Show Material materials with Streckgrenze of 690 MPa | |
540.0 °C | 220 MPa Show Material materials with Streckgrenze of 220 MPa | ||
650.0 °C | 110 MPa Show Material materials with Streckgrenze of 110 MPa | ||
Zugfestigkeit | 20.0 °C | 920 MPa Show Material materials with Zugfestigkeit of 920 MPa | |
540.0 °C | 270 MPa Show Material materials with Zugfestigkeit of 270 MPa | ||
650.0 °C | 130 MPa Show Material materials with Zugfestigkeit of 130 MPa | ||
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1E-5 - 1.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1E-5 - 1.5E-5 1/K | Typical for Martensitic Stainless Steel |
Schmelzpunkt | 1370 - 1530 °C Show Material materials with Schmelzpunkt of 1370 - 1530 °C | Typical for Martensitic Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) | Typical for Martensitic Stainless Steel |
Wärmeleitfähigkeit | 23.0 °C | 14 - 31 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 14 - 31 W/(m·K) | Typical for Martensitic Stainless Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 6E-7 Ω·m Show Material materials with spezifischer Widerstand of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 1.85 - 2.5 % Show Material materials with Chrom of 1.85 - 2.5 % |
Eisen | 91.85 - 94 % Show Material materials with Eisen of 91.85 - 94 % |
Kohlenstoff | 0.35 - 0.45 % Show Material materials with Kohlenstoff of 0.35 - 0.45 % |
Kupfer | 0.25 % Show Material materials with Kupfer of 0.25 % |
Mangan | 0.2 - 0.4 % Show Material materials with Mangan of 0.2 - 0.4 % |
Molybdän | 0.1 % Show Material materials with Molybdän of 0.1 % |
Nickel | 0.25 % Show Material materials with Nickel of 0.25 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.04 % Show Material materials with Schwefel of 0.04 % |
Silizium | 3.6 - 4.2 % Show Material materials with Silizium of 3.6 - 4.2 % |