Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 23.0 °C | 68 % Show Material materials with Flächenreduzierung of 68 % | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 23.0 °C | 710 MPa Show Material materials with Streckgrenze of 710 MPa | |
Zugfestigkeit | 23.0 °C | 900 MPa Show Material materials with Zugfestigkeit of 900 MPa |
Chemical properties
Property | Value |
---|---|
Eisen | 98.61 - 100 % Show Material materials with Eisen of 98.61 - 100 % |
Kohlenstoff | 0.39 % Show Material materials with Kohlenstoff of 0.39 % |
Mangan | 0.75 % Show Material materials with Mangan of 0.75 % |
Silizium | 0.25 % Show Material materials with Silizium of 0.25 % |