Mechanisch
Property | Temperature | Value |
---|---|---|
Flächenreduzierung | 20.0 °C | 5 % Show Material materials with Flächenreduzierung of 5 % |
760.0 °C | 23 % Show Material materials with Flächenreduzierung of 23 % | |
Zugfestigkeit | 20.0 °C | 770 MPa Show Material materials with Zugfestigkeit of 770 MPa |
760.0 °C | 520 MPa Show Material materials with Zugfestigkeit of 520 MPa | |
Chemical properties
Property | Value |
---|---|
Bor | 1.5E-3 % Show Material materials with Bor of 1.5E-3 % |
Chrom | 19 % Show Material materials with Chrom of 19 % |
Eisen | 66 - 100 % Show Material materials with Eisen of 66 - 100 % |
Kohlenstoff | 0.4 % Show Material materials with Kohlenstoff of 0.4 % |
Mangan | 6.5 % Show Material materials with Mangan of 6.5 % |
Nickel | 8 % Show Material materials with Nickel of 8 % |
Niobium | 0.1 % Show Material materials with Niobium of 0.1 % |