Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A5 | 23.0 °C | 10 - 25 % Show Material materials with Dehnung A5 of 10 - 25 % | |
Elastizitätsmodul | 23.0 °C | 205 GPa Show Material materials with Elastizitätsmodul of 205 GPa | |
Flächenreduzierung | 23.0 °C | 6 - 25 % Show Material materials with Flächenreduzierung of 6 - 25 % | |
Härte, Rockwell C | 23.0 °C | 30 [-] Show Material materials with Härte, Rockwell C of 30 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Austenitic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Austenitic Stainless Steel |
Streckgrenze | 23.0 °C | 580 - 880 MPa Show Material materials with Streckgrenze of 580 - 880 MPa | |
Zugfestigkeit | 23.0 °C | 950 - 1190 MPa Show Material materials with Zugfestigkeit of 950 - 1190 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 1.55E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.55E-5 1/K | The mentioned values are between 20°C and the mentioned temperature |
300.0 °C | 1.75E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.75E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
500.0 °C | 1.85E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.85E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
700.0 °C | 1.88E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.88E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
Schmelzpunkt | 1230 - 1480 °C Show Material materials with Schmelzpunkt of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 500 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 500 J/(kg·K) | |
Wärmeleitfähigkeit | 23.0 °C | 14.5 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 14.5 W/(m·K) |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 8.5E-7 Ω·m Show Material materials with spezifischer Widerstand of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value | Comment |
---|---|---|
Chrom | 20 - 22 % Show Material materials with Chrom of 20 - 22 % | |
Eisen | 59.4 - 66.85 % Show Material materials with Eisen of 59.4 - 66.85 % | Balance |
Kohlenstoff | 0.45 - 0.55 % Show Material materials with Kohlenstoff of 0.45 - 0.55 % | |
Mangan | 8 - 10 % Show Material materials with Mangan of 8 - 10 % | |
Nickel | 3.5 - 5.5 % Show Material materials with Nickel of 3.5 - 5.5 % | |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % | |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % | |
Silizium | 0.45 % Show Material materials with Silizium of 0.45 % | |
Stickstoff | 0.4 - 0.6 % Show Material materials with Stickstoff of 0.4 - 0.6 % | |
Wolfram | 0.8 - 1.5 % Show Material materials with Wolfram of 0.8 - 1.5 % |