Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.13 g/cm³ Show Material materials with Dichte of 8.13 g/cm³ |
Mechanisch
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 760.0 °C | 1.53E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.53E-5 1/K | The mentioned value is between 20°C and the mentioned temperature |
Chemical properties
Property | Value |
---|---|
Aluminium | 1 % Show Material materials with Aluminium of 1 % |
Chrom | 27.8 % Show Material materials with Chrom of 27.8 % |
Eisen | 60.2 - 100 % Show Material materials with Eisen of 60.2 - 100 % |
Kohlenstoff | 0.1 % Show Material materials with Kohlenstoff of 0.1 % |
Mangan | 8.5 % Show Material materials with Mangan of 8.5 % |
Nickel | 0.4 % Show Material materials with Nickel of 0.4 % |