Mechanisch
Chemical properties
Property | Value |
---|---|
Aluminium | 0.5 % Show Material materials with Aluminium of 0.5 % |
Bor | 0.05 % Show Material materials with Bor of 0.05 % |
Chrom | 19 % Show Material materials with Chrom of 19 % |
Eisen | 21.21 - 100 % Show Material materials with Eisen of 21.21 - 100 % |
Kohlenstoff | 0.04 % Show Material materials with Kohlenstoff of 0.04 % |
Mangan | 0.2 % Show Material materials with Mangan of 0.2 % |
Nickel | 52.5 % Show Material materials with Nickel of 52.5 % |
Silizium | 0.3 % Show Material materials with Silizium of 0.3 % |