Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Chrom | 1 - 1.45 % Show Material materials with Chrom of 1 - 1.45 % |
Kohlenstoff | 0.07 - 0.13 % Show Material materials with Kohlenstoff of 0.07 - 0.13 % |
Kupfer | 0.3 % Show Material materials with Kupfer of 0.3 % |
Mangan | 0.4 - 0.7 % Show Material materials with Mangan of 0.4 - 0.7 % |
Molybdän | 0.08 - 0.15 % Show Material materials with Molybdän of 0.08 - 0.15 % |
Nickel | 2.95 - 3.55 % Show Material materials with Nickel of 2.95 - 3.55 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Sauerstoff | 2E-3 % Show Material materials with Sauerstoff of 2E-3 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.15 - 0.35 % Show Material materials with Silizium of 0.15 - 0.35 % |