Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 9.6 % Show Material materials with Dehnung of 9.6 % | Predicted Value, A80 | ||||
10.3 % Show Material materials with Dehnung of 10.3 % | Predicted Value, A200 | |||||
10.6 % Show Material materials with Dehnung of 10.6 % | Predicted Value, Transverse | |||||
11.2 % Show Material materials with Dehnung of 11.2 % | Predicted Value, A50 | |||||
16.1 % Show Material materials with Dehnung of 16.1 % | Predicted Value, A5 | |||||
19.3 % Show Material materials with Dehnung of 19.3 % | Predicted Value, A80 Transverse | |||||
20 °C | 13 % Show Material materials with Dehnung of 13 % | quenched and tempered (+QT) | ISO 683-2, EN 10083-3 | Bar, Forging, Sheet, Strip, Flat | ||
Elastizitätsmodul | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel | ||||
Flächenreduzierung | 42.7 % Show Material materials with Flächenreduzierung of 42.7 % | Predicted Value, Transverse | ||||
20 °C | 50 % Show Material materials with Flächenreduzierung of 50 % | quenched and tempered (+QT) | ISO 683-2, EN 10083-3 | Bar, Forging, Sheet, Strip, Flat | ||
Härte, Brinell | 260 [-] Show Material materials with Härte, Brinell of 260 [-] | Predicted Value, Transverse | ||||
Poissonzahl | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel | ||||
Scherfestigkeit | 532 MPa Show Material materials with Scherfestigkeit of 532 MPa | Predicted Value | ||||
Schubmodule | 80.3 GPa Show Material materials with Schubmodule of 80.3 GPa | Predicted Value | ||||
Streckgrenze | 318.7 MPa Show Material materials with Streckgrenze of 318.7 MPa | Predicted Value, RP1 | ||||
326.9 MPa Show Material materials with Streckgrenze of 326.9 MPa | Predicted Value, RP1 Transverse | |||||
347.3 MPa Show Material materials with Streckgrenze of 347.3 MPa | Predicted Value, RP05 | |||||
517.9 MPa Show Material materials with Streckgrenze of 517.9 MPa | Predicted Value, Transverse | |||||
573.8 MPa Show Material materials with Streckgrenze of 573.8 MPa | Predicted Value, RP02 Transverse | |||||
745.8 MPa Show Material materials with Streckgrenze of 745.8 MPa | Predicted Value, RP002 | |||||
866.7 MPa Show Material materials with Streckgrenze of 866.7 MPa | Predicted Value, RP02 | |||||
20 °C | 750 MPa Show Material materials with Streckgrenze of 750 MPa | quenched and tempered (+QT) | ISO 683-2, EN 10083-3 | Bar, Forging, Sheet, Strip, Flat | ||
20 °C | 800 MPa Show Material materials with Streckgrenze of 800 MPa | quenched and tempered (+QT) | ISO 683-2, EN 10083-3 | Bar, Forging, Sheet, Strip, Flat | ||
20 °C | 850 MPa Show Material materials with Streckgrenze of 850 MPa | quenched and tempered (+QT) | ISO 683-2, EN 10083-3 | Bar, Forging, Sheet, Strip, Flat | ||
Zugfestigkeit | 20 °C | 900 - 1300 MPa Show Material materials with Zugfestigkeit of 900 - 1300 MPa | quenched and tempered (+QT) | ISO 683-2, EN 10083-3 | Bar, Forging, Sheet, Strip, Flat | |
20 °C | 900 - 1200 MPa Show Material materials with Zugfestigkeit of 900 - 1200 MPa | quenched and tempered (+QT) | ISO 683-2, EN 10083-3 | Bar, Forging, Sheet, Strip, Flat | ||
20 °C | 900 - 1100 MPa Show Material materials with Zugfestigkeit of 900 - 1100 MPa | quenched and tempered (+QT) | ISO 683-2, EN 10083-3 | Bar, Forging, Sheet, Strip, Flat | ||
20 °C | 950 - 1300 MPa Show Material materials with Zugfestigkeit of 950 - 1300 MPa | quenched and tempered (+QT) | ISO 683-2, EN 10083-3 | Bar, Forging, Sheet, Strip, Flat | ||
20 °C | 950 - 1200 MPa Show Material materials with Zugfestigkeit of 950 - 1200 MPa | quenched and tempered (+QT) | ISO 683-2, EN 10083-3 | Bar, Forging, Sheet, Strip, Flat | ||
20 °C | 950 - 1100 MPa Show Material materials with Zugfestigkeit of 950 - 1100 MPa | quenched and tempered (+QT) | ISO 683-2, EN 10083-3 | Bar, Forging, Sheet, Strip, Flat | ||
20 °C | 1050 - 1300 MPa Show Material materials with Zugfestigkeit of 1050 - 1300 MPa | quenched and tempered (+QT) | ISO 683-2, EN 10083-3 | Bar, Forging, Sheet, Strip, Flat | ||
20 °C | 1050 - 1200 MPa Show Material materials with Zugfestigkeit of 1050 - 1200 MPa | quenched and tempered (+QT) | ISO 683-2, EN 10083-3 | Bar, Forging, Sheet, Strip, Flat | ||
20 °C | 1050 - 1100 MPa Show Material materials with Zugfestigkeit of 1050 - 1100 MPa | quenched and tempered (+QT) | ISO 683-2, EN 10083-3 | Bar, Forging, Sheet, Strip, Flat |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 12.21 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 12.21 1/K | Predicted Value |
Max. Betriebstemperatur | 287.1 °C Show Material materials with Max. Betriebstemperatur of 287.1 °C | Predicted Value, Long |
Spezifische Wärmekapazität | 456.8 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 456.8 J/(kg·K) | Predicted Value |
Wärmeleitfähigkeit | 36.54 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 36.54 W/(m·K) | Predicted Value |
Elektrisch
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Bor | 0.0008 - 0.005 % Show Material materials with Bor of 0.0008 - 0.005 % | quenched and tempered (+QT) | ISO 683-2, EN 10083-3 | Bar, Forging, Sheet, Strip, Flat |
0.001 - 0.005 % Show Material materials with Bor of 0.001 - 0.005 % | quenched and tempered (+QT) | EN 10083-3, ISO 683-2 | Bar, Forging, Sheet, Strip, Flat | |
Chrom | 0.3 - 0.6 % Show Material materials with Chrom of 0.3 - 0.6 % | quenched and tempered (+QT) | ISO 683-2, EN 10083-3 | Bar, Forging, Sheet, Strip, Flat |
Kohlenstoff | 0.3 - 0.36 % Show Material materials with Kohlenstoff of 0.3 - 0.36 % | quenched and tempered (+QT) | ISO 683-2, EN 10083-3 | Bar, Forging, Sheet, Strip, Flat |
Kupfer | 0.4 % Show Material materials with Kupfer of 0.4 % | quenched and tempered (+QT) | ISO 683-2, EN 10083-3 | Bar, Forging, Sheet, Strip, Flat |
Mangan | 1.2 - 1.5 % Show Material materials with Mangan of 1.2 - 1.5 % | quenched and tempered (+QT) | ISO 683-2, EN 10083-3 | Bar, Forging, Sheet, Strip, Flat |
Phosphor | 0.025 % Show Material materials with Phosphor of 0.025 % | quenched and tempered (+QT) | ISO 683-2, EN 10083-3 | Bar, Forging, Sheet, Strip, Flat |
Schwefel | 0.035 % Show Material materials with Schwefel of 0.035 % | quenched and tempered (+QT) | ISO 683-2, EN 10083-3 | Bar, Forging, Sheet, Strip, Flat |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % | quenched and tempered (+QT) | ISO 683-2, EN 10083-3 | Bar, Forging, Sheet, Strip, Flat |