Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Chromium Molybdenum Steel |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 15.0 % Show Material materials with Dehnung of 15.0 % | Predicted Value, A200 | ||||
16.4 % Show Material materials with Dehnung of 16.4 % | Predicted Value, A80 | |||||
18.9 % Show Material materials with Dehnung of 18.9 % | Predicted Value, A5 | |||||
20.1 % Show Material materials with Dehnung of 20.1 % | Predicted Value, A80 Transverse | |||||
23.6 % Show Material materials with Dehnung of 23.6 % | Predicted Value, A50 | |||||
20 °C | 18 % Show Material materials with Dehnung of 18 % | quenched and tempered (+QT) | EN 10028-2 | Flat | Transverse | |
20 °C | 18 % Show Material materials with Dehnung of 18 % | quenched and tempered (+QT) | EN 10028-2 | Flat | ||
Elastizitätsmodul | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Chromium Molybdenum Steel | ||||
Flächenreduzierung | 43.4 % Show Material materials with Flächenreduzierung of 43.4 % | Predicted Value | ||||
43.5 % Show Material materials with Flächenreduzierung of 43.5 % | Predicted Value, Transverse | |||||
Härte, Brinell | 258 [-] Show Material materials with Härte, Brinell of 258 [-] | Predicted Value, Transverse | ||||
Poissonzahl | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Chromium Molybdenum Steel | ||||
Scherfestigkeit | 677.8 MPa Show Material materials with Scherfestigkeit of 677.8 MPa | Predicted Value | ||||
Schubmodule | 79.1 GPa Show Material materials with Schubmodule of 79.1 GPa | Predicted Value | ||||
Streckgrenze | 286.7 MPa Show Material materials with Streckgrenze of 286.7 MPa | Predicted Value, RP1 | ||||
327.8 MPa Show Material materials with Streckgrenze of 327.8 MPa | Predicted Value, RP1 Transverse | |||||
479.2 MPa Show Material materials with Streckgrenze of 479.2 MPa | Predicted Value, RP05 | |||||
491.2 MPa Show Material materials with Streckgrenze of 491.2 MPa | Predicted Value, RP02 Transverse | |||||
567.4 MPa Show Material materials with Streckgrenze of 567.4 MPa | Predicted Value, RP002 | |||||
20 °C | 415 MPa Show Material materials with Streckgrenze of 415 MPa | quenched and tempered (+QT) | EN 10028-2 | Flat | Transverse | |
20 °C | 415 MPa Show Material materials with Streckgrenze of 415 MPa | quenched and tempered (+QT) | EN 10028-2 | Flat | ||
50 °C | 405 MPa Show Material materials with Streckgrenze of 405 MPa | quenched and tempered (+QT) | EN 10028-2 | Flat | RP02 | |
100 °C | 390 MPa Show Material materials with Streckgrenze of 390 MPa | quenched and tempered (+QT) | EN 10028-2 | Flat | RP02 | |
150 °C | 370 MPa Show Material materials with Streckgrenze of 370 MPa | quenched and tempered (+QT) | EN 10028-2 | Flat | RP02 | |
200 °C | 365 MPa Show Material materials with Streckgrenze of 365 MPa | quenched and tempered (+QT) | EN 10028-2 | Flat | RP02 | |
250 °C | 360 MPa Show Material materials with Streckgrenze of 360 MPa | quenched and tempered (+QT) | EN 10028-2 | Flat | RP02 | |
300 °C | 355 MPa Show Material materials with Streckgrenze of 355 MPa | quenched and tempered (+QT) | EN 10028-2 | Flat | RP02 | |
350 °C | 352 MPa Show Material materials with Streckgrenze of 352 MPa | quenched and tempered (+QT) | EN 10028-2 | Flat | RP02 | |
400 °C | 350 MPa Show Material materials with Streckgrenze of 350 MPa | quenched and tempered (+QT) | EN 10028-2 | Flat | RP02 | |
450 °C | 340 MPa Show Material materials with Streckgrenze of 340 MPa | quenched and tempered (+QT) | EN 10028-2 | Flat | RP02 | |
Zugfestigkeit | 20 °C | 580 - 760 MPa Show Material materials with Zugfestigkeit of 580 - 760 MPa | quenched and tempered (+QT) | EN 10028-2 | Flat | Transverse |
20 °C | 580 - 760 MPa Show Material materials with Zugfestigkeit of 580 - 760 MPa | quenched and tempered (+QT) | EN 10028-2 | Flat |
Thermisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 1.1e-05 - 1.4e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.1e-05 - 1.4e-05 1/K | Typical for Chromium Molybdenum Steel | |||
Max. Betriebstemperatur | 20 - 450 °C Show Material materials with Max. Betriebstemperatur of 20 - 450 °C | quenched and tempered (+QT) | EN 10028-2 | Flat | Long |
450 °C Show Material materials with Max. Betriebstemperatur of 450 °C | quenched and tempered (+QT) | EN 10028-2 | Flat | Long | |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel | |||
Spezifische Wärmekapazität | 448 - 502 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel | |||
Wärmeleitfähigkeit | 36 - 43 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Elektrisch
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Bor | 0.002 % Show Material materials with Bor of 0.002 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Chrom | 2 - 2.5 % Show Material materials with Chrom of 2 - 2.5 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Kalzium | 0.015 % Show Material materials with Kalzium of 0.015 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Kohlenstoff | 0.11 - 0.15 % Show Material materials with Kohlenstoff of 0.11 - 0.15 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Kupfer | 0.2 % Show Material materials with Kupfer of 0.2 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Mangan | 0.3 - 0.6 % Show Material materials with Mangan of 0.3 - 0.6 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Molybdän | 0.9 - 1.1 % Show Material materials with Molybdän of 0.9 - 1.1 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Nickel | 0.25 % Show Material materials with Nickel of 0.25 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Niobium | 0.07 % Show Material materials with Niobium of 0.07 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Phosphor | 0.015 % Show Material materials with Phosphor of 0.015 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Schwefel | 0.005 % Show Material materials with Schwefel of 0.005 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
0.01 % Show Material materials with Schwefel of 0.01 % | quenched and tempered (+QT) | EN 10028-2 | Flat | |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Stickstoff | 0.012 % Show Material materials with Stickstoff of 0.012 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Titan | 0.03 % Show Material materials with Titan of 0.03 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Vanadium | 0.25 - 0.35 % Show Material materials with Vanadium of 0.25 - 0.35 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |