Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 18 % Show Material materials with Dehnung A50 of 18 % |
Flächenreduzierung | 20.0 °C | 33 % Show Material materials with Flächenreduzierung of 33 % |
Härte, Brinell | 20.0 °C | 137 - 197 [-] Show Material materials with Härte, Brinell of 137 - 197 [-] |
Yield Strength Rp0.2, short transverse | 20.0 °C | 250 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 250 MPa |
Zugfestigkeit | 20.0 °C | 485 - 655 MPa Show Material materials with Zugfestigkeit of 485 - 655 MPa |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 0.3 % Show Material materials with Kohlenstoff of 0.3 % |
Mangan | 0.4 - 1.05 % Show Material materials with Mangan of 0.4 - 1.05 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 0.15 - 0.35 % Show Material materials with Silizium of 0.15 - 0.35 % |