Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 17 % Show Material materials with Dehnung A50 of 17 % |
Flächenreduzierung | 20.0 °C | 30 % Show Material materials with Flächenreduzierung of 30 % |
Härte, Brinell | 20.0 °C | 156 - 207 [-] Show Material materials with Härte, Brinell of 156 - 207 [-] |
Yield Strength Rp0.2, short transverse | 20.0 °C | 260 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 260 MPa |
Zugfestigkeit | 20.0 °C | 515 - 690 MPa Show Material materials with Zugfestigkeit of 515 - 690 MPa |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 0.35 % Show Material materials with Kohlenstoff of 0.35 % |
Mangan | 0.8 - 1.35 % Show Material materials with Mangan of 0.8 - 1.35 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 0.15 - 0.35 % Show Material materials with Silizium of 0.15 - 0.35 % |