Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 23.0 °C | 23 % Show Material materials with Dehnung A50 of 23 % |
Elongation A200 | 23.0 °C | 20 % Show Material materials with Elongation A200 of 20 % |
Streckgrenze | 23.0 °C | 230 MPa Show Material materials with Streckgrenze of 230 MPa |
Zugfestigkeit | 23.0 °C | 415 - 550 MPa Show Material materials with Zugfestigkeit of 415 - 550 MPa |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 0.27 % Show Material materials with Kohlenstoff of 0.27 % |
Kupfer | 0.2 % Show Material materials with Kupfer of 0.2 % |
Mangan | 0.9 % Show Material materials with Mangan of 0.9 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % |