Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 40 % Show Material materials with Dehnung of 40 % | |
Dehnung A50 | 20.0 °C | 32 - 40 % Show Material materials with Dehnung A50 of 32 - 40 % | |
Dehnung A80 | 20.0 °C | 30 - 38 % Show Material materials with Dehnung A80 of 30 - 38 % | |
Elastizitätsmodul | 20.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Low Carbon Steel |
Härte, Vickers | 20.0 °C | 105 - 115 [-] Show Material materials with Härte, Vickers of 105 - 115 [-] | |
Poissonzahl | 20.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Low Carbon Steel |
Streckgrenze | 20.0 °C | 140 - 250 MPa Show Material materials with Streckgrenze of 140 - 250 MPa | |
Zugfestigkeit | 20.0 °C | 35 - 350 MPa Show Material materials with Zugfestigkeit of 35 - 350 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 1.32E-5 - 1.38E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32E-5 - 1.38E-5 1/K | Typical for Low Carbon Steel |
Schmelzpunkt | 1480 - 1526 °C Show Material materials with Schmelzpunkt of 1480 - 1526 °C | Typical for Low Carbon Steel |
Magnetisch
Property | Value | Comment |
---|---|---|
Curie-Temperatur | 770 °C Show Material materials with Curie-Temperatur of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 0.08 % Show Material materials with Kohlenstoff of 0.08 % |
Mangan | 0.4 % Show Material materials with Mangan of 0.4 % |
Phosphor | 0.03 - 0.04 % Show Material materials with Phosphor of 0.03 - 0.04 % |
Schwefel | 0.03 - 0.035 % Show Material materials with Schwefel of 0.03 - 0.035 % |