Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Medium Carbon Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Medium Carbon Steel |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Medium Carbon Steel |
Schubmodule | 23.0 °C | 75 - 80 GPa Show Material materials with Schubmodule of 75 - 80 GPa | Typical for Carbon Steel |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.32E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32E-5 1/K | Typical for Medium Carbon Steel |
Max. Betriebstemperatur | 500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel | |
Schmelzpunkt | 1380 - 1514 °C Show Material materials with Schmelzpunkt of 1380 - 1514 °C | Typical for Medium Carbon Steel | |
Spezifische Wärmekapazität | 23.0 °C | 470 - 520 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 470 - 520 J/(kg·K) | Typical for Medium Carbon Steel |
Wärmeleitfähigkeit | 23.0 °C | 21 - 52 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 21 - 52 W/(m·K) | Typical for Medium Carbon Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with spezifischer Widerstand of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Chemical properties
Property | Value |
---|---|
Eisen | 98.17 - 98.8 % Show Material materials with Eisen of 98.17 - 98.8 % |
Kohlenstoff | 0.45 - 0.51 % Show Material materials with Kohlenstoff of 0.45 - 0.51 % |
Mangan | 0.6 - 0.9 % Show Material materials with Mangan of 0.6 - 0.9 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.035 % Show Material materials with Schwefel of 0.035 % |
Silizium | 0.15 - 0.35 % Show Material materials with Silizium of 0.15 - 0.35 % |