Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 0.7 - 1 % Show Material materials with Chrom of 0.7 - 1 % |
Eisen | 94.26 - 95.68 % Show Material materials with Eisen of 94.26 - 95.68 % |
Kohlenstoff | 0.12 - 0.18 % Show Material materials with Kohlenstoff of 0.12 - 0.18 % |
Mangan | 0.35 - 0.65 % Show Material materials with Mangan of 0.35 - 0.65 % |
Nickel | 3 - 3.5 % Show Material materials with Nickel of 3 - 3.5 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 0.15 - 0.35 % Show Material materials with Silizium of 0.15 - 0.35 % |