Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Duplex Stainless Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 200 GPa Show Material materials with Elastizitätsmodul of 200 GPa | Typical for Duplex Stainless Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Duplex Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Duplex Stainless Steel |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1E-5 1/K | Typical for Duplex Stainless Steel |
Max. Betriebstemperatur | 300 °C Show Material materials with Max. Betriebstemperatur of 300 °C | Typical for Duplex Stainless Steel | |
Schmelzpunkt | 1375 - 1450 °C Show Material materials with Schmelzpunkt of 1375 - 1450 °C | Typical for Duplex Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 440 - 502 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 440 - 502 J/(kg·K) | Typical for Duplex Stainless Steel |
Wärmeleitfähigkeit | 23.0 °C | 13 - 30 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 13 - 30 W/(m·K) | Typical for Duplex Stainless Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 23 - 28 % Show Material materials with Chrom of 23 - 28 % |
Eisen | 60.35 - 73 % Show Material materials with Eisen of 60.35 - 73 % |
Kohlenstoff | 0.08 % Show Material materials with Kohlenstoff of 0.08 % |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % |
Molybdän | 1 - 3 % Show Material materials with Molybdän of 1 - 3 % |
Nickel | 3 - 6 % Show Material materials with Nickel of 3 - 6 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |