Chemical properties
Property | Value |
---|---|
Chrom | 25 - 27.5 % Show Material materials with Chrom of 25 - 27.5 % |
Kohlenstoff | 0.01 % Show Material materials with Kohlenstoff of 0.01 % |
Kupfer | 0.2 % Show Material materials with Kupfer of 0.2 % |
Mangan | 0.4 % Show Material materials with Mangan of 0.4 % |
Molybdän | 0.75 - 1.5 % Show Material materials with Molybdän of 0.75 - 1.5 % |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % |
Niobium | 0.05 - 0.2 % Show Material materials with Niobium of 0.05 - 0.2 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.012 % Show Material materials with Schwefel of 0.012 % |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % |
Stickstoff | 0.02 % Show Material materials with Stickstoff of 0.02 % |