Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Manganese Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Manganese Steel |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Manganese Steel |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.33E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.33E-5 1/K | Typical for Manganese Steel |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Manganese Steel | |
Spezifische Wärmekapazität | 23.0 °C | 510 - 553 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 510 - 553 J/(kg·K) | Typical for Manganese Steel |
Wärmeleitfähigkeit | 23.0 °C | 14 - 16 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 14 - 16 W/(m·K) | Typical for Manganese Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % |
Chrom | 0.02 % Show Material materials with Chrom of 0.02 % |
Eisen | balance |
Kohlenstoff | 0.4 - 0.48 % Show Material materials with Kohlenstoff of 0.4 - 0.48 % |
Kupfer | 0.02 % Show Material materials with Kupfer of 0.02 % |
Mangan | 1.35 - 1.65 % Show Material materials with Mangan of 1.35 - 1.65 % |
Molybdän | 0.02 % Show Material materials with Molybdän of 0.02 % |
Nickel | 0.02 % Show Material materials with Nickel of 0.02 % |
Niobium | 0.08 % Show Material materials with Niobium of 0.08 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.24 - 0.33 % Show Material materials with Schwefel of 0.24 - 0.33 % |
Silizium | 0.02 % Show Material materials with Silizium of 0.02 % |
Titan | 0.08 % Show Material materials with Titan of 0.08 % |
Vanadium | 0.08 % Show Material materials with Vanadium of 0.08 % |