Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Chromium Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 11 - 14 % Show Material materials with Dehnung of 11 - 14 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Chromium Steel |
Flächenreduzierung | 20.0 °C | 40 - 50 % Show Material materials with Flächenreduzierung of 40 - 50 % | |
Hardness, Rockwell F | 20.0 °C | 54 [-] Show Material materials with Hardness, Rockwell F of 54 [-] | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Chromium Steel |
Streckgrenze | 20.0 °C | 560 - 780 MPa Show Material materials with Streckgrenze of 560 - 780 MPa | |
Zugfestigkeit | 20.0 °C | 780 - 1180 MPa Show Material materials with Zugfestigkeit of 780 - 1180 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 9.4E-6 - 1.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9.4E-6 - 1.5E-5 1/K | Typical for Chromium Steel |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Chromium Steel | |
Spezifische Wärmekapazität | 23.0 °C | 440 - 494 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 440 - 494 J/(kg·K) | Typical for Chromium Steel |
Wärmeleitfähigkeit | 23.0 °C | 23 - 50 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 23 - 50 W/(m·K) | Typical for Chromium Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 0.9 - 1.2 % Show Material materials with Chrom of 0.9 - 1.2 % |
Kohlenstoff | 0.38 - 0.44 % Show Material materials with Kohlenstoff of 0.38 - 0.44 % |
Mangan | 0.5 - 0.8 % Show Material materials with Mangan of 0.5 - 0.8 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.035 % Show Material materials with Schwefel of 0.035 % |
Silizium | 0.15 - 0.4 % Show Material materials with Silizium of 0.15 - 0.4 % |