Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 11 - 13 % Show Material materials with Dehnung of 11 - 13 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung | 20.0 °C | 25 - 30 % Show Material materials with Flächenreduzierung of 25 - 30 % | |
Hardness, Rockwell F | 20.0 °C | 60 [-] Show Material materials with Hardness, Rockwell F of 60 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 20.0 °C | 480 - 560 MPa Show Material materials with Streckgrenze of 480 - 560 MPa | |
Zugfestigkeit | 20.0 °C | 740 - 930 MPa Show Material materials with Zugfestigkeit of 740 - 930 MPa |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 0.68 - 0.75 % Show Material materials with Kohlenstoff of 0.68 - 0.75 % |
Mangan | 0.2 - 0.35 % Show Material materials with Mangan of 0.2 - 0.35 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.035 % Show Material materials with Schwefel of 0.035 % |
Silizium | 0.15 - 0.35 % Show Material materials with Silizium of 0.15 - 0.35 % |