Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Chromium Vanadium Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 20.0 °C | 206 GPa Show Material materials with Elastizitätsmodul of 206 GPa | |
Flächenreduzierung | 20.0 °C | 40 - 50 % Show Material materials with Flächenreduzierung of 40 - 50 % | |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Chromium Vanadium Steel |
Schubmodule | 20.0 °C | 79.5 GPa Show Material materials with Schubmodule of 79.5 GPa | |
Zugfestigkeit | 20.0 °C | 1390 - 2060 MPa Show Material materials with Zugfestigkeit of 1390 - 2060 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.2E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.2E-5 1/K | Typical for Chromium Vanadium Steel |
Max. Betriebstemperatur, lang | -60 - 200 °C Show Material materials with Max. Betriebstemperatur, lang of -60 - 200 °C | ||
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Chromium Vanadium Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 0.4 - 0.6 % Show Material materials with Chrom of 0.4 - 0.6 % |
Kohlenstoff | 0.62 - 0.72 % Show Material materials with Kohlenstoff of 0.62 - 0.72 % |
Kupfer | 0.06 % Show Material materials with Kupfer of 0.06 % |
Mangan | 0.5 - 0.9 % Show Material materials with Mangan of 0.5 - 0.9 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % |
Silizium | 0.15 - 0.3 % Show Material materials with Silizium of 0.15 - 0.3 % |
Vanadium | 0.15 - 0.25 % Show Material materials with Vanadium of 0.15 - 0.25 % |
Technological properties
Property | ||
---|---|---|
Features | Spring |