Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.6 g/cm³ Show Material materials with Dichte of 7.6 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 195 GPa Show Material materials with Elastizitätsmodul of 195 GPa | Typical for Austenitic Stainless Steel |
Härte, Brinell | 20.0 °C | 200 - 300 [-] Show Material materials with Härte, Brinell of 200 - 300 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Austenitic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Austenitic Stainless Steel |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 400.0 °C | 1.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.3E-5 1/K | |
800.0 °C | 1.45E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.45E-5 1/K | ||
1000.0 °C | 1.65E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.65E-5 1/K | ||
Max. Betriebstemperatur, lang | 0 - 1100 °C Show Material materials with Max. Betriebstemperatur, lang of 0 - 1100 °C | ||
Schmelzpunkt | 1230 - 1480 °C Show Material materials with Schmelzpunkt of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Spezifische Wärmekapazität | 20.0 °C | 500 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 500 J/(kg·K) | |
Wärmeleitfähigkeit | 20.0 °C | 16.7 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 16.7 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 8E-7 Ω·m Show Material materials with spezifischer Widerstand of 8E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Chrom | 25 - 28 % Show Material materials with Chrom of 25 - 28 % |
Kohlenstoff | 0.35 - 0.5 % Show Material materials with Kohlenstoff of 0.35 - 0.5 % |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % |
Nickel | 3.5 - 5.5 % Show Material materials with Nickel of 3.5 - 5.5 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |