Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.3 g/cm³ Show Material materials with Dichte of 7.3 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 8 % Show Material materials with Dehnung of 8 % | |
Elastizitätsmodul | 23.0 °C | 220 GPa Show Material materials with Elastizitätsmodul of 220 GPa | Typical for Ferritic Stainless Steel |
Elongation A100 | 20.0 °C | 8 - 18 % Show Material materials with Elongation A100 of 8 - 18 % | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Ferritic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Ferritic Stainless Steel |
Zugfestigkeit | 20.0 °C | 600 MPa Show Material materials with Zugfestigkeit of 600 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 200.0 °C | 1.1E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.1E-5 1/K | |
400.0 °C | 1.2E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.2E-5 1/K | ||
600.0 °C | 1.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.3E-5 1/K | ||
800.0 °C | 1.4E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.4E-5 1/K | ||
1000.0 °C | 1.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.5E-5 1/K | ||
Max. Betriebstemperatur, lang | 1250 - 1350 °C Show Material materials with Max. Betriebstemperatur, lang of 1250 - 1350 °C | ||
Schmelzpunkt | 1425 - 1530 °C Show Material materials with Schmelzpunkt of 1425 - 1530 °C | Typical for Ferritic Stainless Steel | |
Spezifische Wärmekapazität | 20.0 °C | 480 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 480 J/(kg·K) | |
1000.0 °C | 650 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 650 J/(kg·K) | ||
Wärmeleitfähigkeit | 20.0 °C | 15 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 15 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
spezifischer Widerstand | 20.0 °C | 1.25E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.25E-6 Ω·m |
100.0 °C | 1.26E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.26E-6 Ω·m | |
200.0 °C | 1.27E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.27E-6 Ω·m | |
300.0 °C | 1.28E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.28E-6 Ω·m | |
400.0 °C | 1.3E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.3E-6 Ω·m | |
500.0 °C | 1.32E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.32E-6 Ω·m | |
600.0 °C | 1.34E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.34E-6 Ω·m | |
700.0 °C | 1.36E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.36E-6 Ω·m | |
800.0 °C | 1.39E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.39E-6 Ω·m | |
900.0 °C | 1.41E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.41E-6 Ω·m | |
1000.0 °C | 1.42E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.42E-6 Ω·m | |
1100.0 °C | 1.44E-6 Ω·m Show Material materials with spezifischer Widerstand of 1.44E-6 Ω·m | |
Chemical properties
Property | Value |
---|---|
Aluminium | 3.5 - 5 % Show Material materials with Aluminium of 3.5 - 5 % |
Chrom | 13 - 15 % Show Material materials with Chrom of 13 - 15 % |
Kohlenstoff | 0.1 % Show Material materials with Kohlenstoff of 0.1 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |