Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 4 % Show Material materials with Dehnung of 4 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Härte, Vickers, 5 | 20.0 °C | 220 [-] Show Material materials with Härte, Vickers, 5 of 220 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 20.0 °C | 700 MPa Show Material materials with Streckgrenze Rp 0,2 of 700 MPa | |
Zugfestigkeit | 20.0 °C | 750 MPa Show Material materials with Zugfestigkeit of 750 MPa |
Chemical properties
Property | Value |
---|---|
Nickel | 50 % Show Material materials with Nickel of 50 % |