Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 21 - 26 % Show Material materials with Dehnung of 21 - 26 % | |
Dehnung A80 | 20.0 °C | 17 - 21 % Show Material materials with Dehnung A80 of 17 - 21 % | |
Dehnung A80, transversal | 20.0 °C | 17 - 21 % Show Material materials with Dehnung A80, transversal of 17 - 21 % | |
Dehnung, transversal | 20.0 °C | 21 - 24 % Show Material materials with Dehnung, transversal of 21 - 24 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Low Carbon Steel |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Low Carbon Steel |
Schubmodule | 23.0 °C | 82 GPa Show Material materials with Schubmodule of 82 GPa | Typical for Low Carbon Steel |
Streckgrenze | 20.0 °C | 175 - 235 MPa Show Material materials with Streckgrenze of 175 - 235 MPa | |
Zugfestigkeit | 20.0 °C | 340 - 510 MPa Show Material materials with Zugfestigkeit of 340 - 510 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.32E-5 - 1.38E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32E-5 - 1.38E-5 1/K | Typical for Low Carbon Steel |
Max. Betriebstemperatur | 500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel | |
Schmelzpunkt | 1480 - 1526 °C Show Material materials with Schmelzpunkt of 1480 - 1526 °C | Typical for Low Carbon Steel | |
Spezifische Wärmekapazität | 23.0 °C | 465 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 465 J/(kg·K) | Typical for Low Carbon Steel |
Wärmeleitfähigkeit | 23.0 °C | 25 - 93 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with spezifischer Widerstand of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Magnetisch
Property | Value | Comment |
---|---|---|
Curie-Temperatur | 770 °C Show Material materials with Curie-Temperatur of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 0.17 % Show Material materials with Kohlenstoff of 0.17 % |
Kupfer | 0.55 % Show Material materials with Kupfer of 0.55 % |
Mangan | 1.4 % Show Material materials with Mangan of 1.4 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.035 % Show Material materials with Schwefel of 0.035 % |
Stickstoff | 0.01 % Show Material materials with Stickstoff of 0.01 % |