Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 25 % Show Material materials with Dehnung of 25 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 20.0 °C | 245 - 255 MPa Show Material materials with Streckgrenze of 245 - 255 MPa | |
Zugfestigkeit | 20.0 °C | 330 - 460 MPa Show Material materials with Zugfestigkeit of 330 - 460 MPa |
Thermisch
Property | Value |
---|---|
Max. Betriebstemperatur, lang | -50 - 0 °C Show Material materials with Max. Betriebstemperatur, lang of -50 - 0 °C |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.015 % Show Material materials with Aluminium of 0.015 % |
Kohlenstoff | 0.1 % Show Material materials with Kohlenstoff of 0.1 % |
Mangan | 1.3 % Show Material materials with Mangan of 1.3 % |
Molybdän | 0.15 % Show Material materials with Molybdän of 0.15 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |
Niobium | 0.05 % Show Material materials with Niobium of 0.05 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.025 % Show Material materials with Schwefel of 0.025 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |
Stickstoff | 0.02 % Show Material materials with Stickstoff of 0.02 % |
Titan | 0.05 % Show Material materials with Titan of 0.05 % |