Mechanisch
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % | min, total |
Bor | 0.002 % Show Material materials with Bor of 0.002 % | max. |
Chrom | 0.3 % Show Material materials with Chrom of 0.3 % | max. |
Kohlenstoff | 0.16 % Show Material materials with Kohlenstoff of 0.16 % | max. |
Kupfer | 0.35 % Show Material materials with Kupfer of 0.35 % | max. |
Mangan | 0.8 - 1.7 % Show Material materials with Mangan of 0.8 - 1.7 % | |
Molybdän | 0.2 % Show Material materials with Molybdän of 0.2 % | max. |
Nickel | 0.7 % Show Material materials with Nickel of 0.7 % | max. |
Niobium | 0.05 % Show Material materials with Niobium of 0.05 % | max. |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % | max. |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % | max. |
Silizium | 0.15 - 0.5 % Show Material materials with Silizium of 0.15 - 0.5 % | |
Vanadium | 0.08 % Show Material materials with Vanadium of 0.08 % | max. |
Technological properties
Property | ||
---|---|---|
Processing methods | The TMCP method consists of rolling reductions and cooling rate controls that result in mechanical properties in the finished plate that are equivalent to those attained using conventional rolling and heat treatment processes, which entail reheating after rolling. | |
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |