Property | Value | Comment |
---|---|---|
Carbon equivalent (CEV) | 0.43 [-] Show Material materials with Carbon equivalent (CEV) of 0.43 [-] | for t ≤ 50 mm plate thickness condition TM |
0.44 [-] Show Material materials with Carbon equivalent (CEV) of 0.44 [-] | for t ≤ 50 mm sections condition TM | |
0.45 [-] Show Material materials with Carbon equivalent (CEV) of 0.45 [-] | for 50 < t ≤100 mm plate thickness condition TM | |
0.45 [-] Show Material materials with Carbon equivalent (CEV) of 0.45 [-] | for t ≤ 50 mm plate thickness condition QT | |
0.46 [-] Show Material materials with Carbon equivalent (CEV) of 0.46 [-] | for t ≤ 50 mm plate thickness condition N/NR | |
0.47 [-] Show Material materials with Carbon equivalent (CEV) of 0.47 [-] | for t ≤ 50 mm sections condition N/NR | |
0.47 [-] Show Material materials with Carbon equivalent (CEV) of 0.47 [-] | for t ≤ 65 mm tabulars condition N/NR | |
0.47 [-] Show Material materials with Carbon equivalent (CEV) of 0.47 [-] | for 100 < t ≤ 250 mm plate thickness condition TM | |
0.47 [-] Show Material materials with Carbon equivalent (CEV) of 0.47 [-] | for 50 < t ≤100 mm plate thickness condition QT | |
0.48 [-] Show Material materials with Carbon equivalent (CEV) of 0.48 [-] | for 50 < t ≤100 mm plate thickness condition N/NR | |
0.49 [-] Show Material materials with Carbon equivalent (CEV) of 0.49 [-] | for 100 < t ≤ 250 mm plate thickness condition QT | |
0.52 [-] Show Material materials with Carbon equivalent (CEV) of 0.52 [-] | for 100 < t ≤ 250 mm plate thickness condition N/NR | |
0.53 [-] Show Material materials with Carbon equivalent (CEV) of 0.53 [-] | for t ≤ 250 or d ≤ 250 mm bars condition N/NR | |
Dichte | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | typical for low carbon steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy, V-notch | -40 °C | 41 J Show Material materials with Charpy impact energy, V-notch of 41 J | |
Charpy impact energy, V-notch, transverse | -40 °C | 27 J Show Material materials with Charpy impact energy, V-notch, transverse of 27 J | |
Dehnung | 18 % Show Material materials with Dehnung of 18 % | min. | |
Elastizitätsmodul | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | typical for low carbon steel | |
Poissonzahl | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | typical for low carbon steel | |
Schubmodule | 82 GPa Show Material materials with Schubmodule of 82 GPa | typical for low carbon steel | |
Zugfestigkeit | 530 - 680 MPa Show Material materials with Zugfestigkeit of 530 - 680 MPa |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.32e-05 - 1.38e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32e-05 - 1.38e-05 1/K | typical for low carbon steel |
Max. Betriebstemperatur | 500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | typical for carbon steel |
Schmelzpunkt | 1480 - 1526 °C Show Material materials with Schmelzpunkt of 1480 - 1526 °C | typical for low carbon steel |
Spezifische Wärmekapazität | 465 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 465 J/(kg·K) | typical for low carbon steel |
Wärmeleitfähigkeit | 25 - 93 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 25 - 93 W/(m·K) | typical for low carbon steel |
Elektrisch
Property | Value | Comment |
---|---|---|
spezifischer Widerstand | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with spezifischer Widerstand of 1.43e-07 - 1.74e-07 Ω·m | typical for carbon steel |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0.018 - 0.2 % Show Material materials with Aluminium of 0.018 - 0.2 % | min., depending on the delivery condition |
Bor | 0.005 % Show Material materials with Bor of 0.005 % | max. |
Chrom | 0.3 - 2 % Show Material materials with Chrom of 0.3 - 2 % | max., depending on the delivery condition |
Kalzium | 0.005 % Show Material materials with Kalzium of 0.005 % | max. |
Kohlenstoff | 0.14 - 0.18 % Show Material materials with Kohlenstoff of 0.14 - 0.18 % | max., depending on the delivery condition |
Kupfer | 0.5 - 0.55 % Show Material materials with Kupfer of 0.5 - 0.55 % | max., depending on the delivery condition |
Mangan | 1 - 1.7 % Show Material materials with Mangan of 1 - 1.7 % | depending on the delivery condition |
Molybdän | 0.1 - 0.7 % Show Material materials with Molybdän of 0.1 - 0.7 % | max., depending on the delivery condition |
Nickel | 0.8 - 3.5 % Show Material materials with Nickel of 0.8 - 3.5 % | max., depending on the delivery condition |
Niobium | 0.05 - 0.06 % Show Material materials with Niobium of 0.05 - 0.06 % | max., depending on the delivery condition |
Phosphor | 0.02 - 0.025 % Show Material materials with Phosphor of 0.02 - 0.025 % | max., depending on the delivery condition |
Sauerstoff | 0.003 - 0.005 % Show Material materials with Sauerstoff of 0.003 - 0.005 % | max., depending on the delivery condition |
Schwefel | 0.01 - 0.02 % Show Material materials with Schwefel of 0.01 - 0.02 % | max., depending on the delivery condition |
Silizium | 0.6 - 0.8 % Show Material materials with Silizium of 0.6 - 0.8 % | max., depending on the delivery condition |
Stickstoff | 0.015 - 0.025 % Show Material materials with Stickstoff of 0.015 - 0.025 % | max., depending on the delivery condition |
Titan | 0.05 % Show Material materials with Titan of 0.05 % | max. |
Vanadium | 0.12 - 0.2 % Show Material materials with Vanadium of 0.12 - 0.2 % | max., depending on the delivery condition |