Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung A50 | 23.0 °C | 20 % Show Material materials with Dehnung A50 of 20 % | |
Elastizitätsmodul | 23.0 °C | 100 - 125 GPa Show Material materials with Elastizitätsmodul of 100 - 125 GPa | Typical for Wrought Copper Brass |
Schubmodule | 23.0 °C | 40 GPa Show Material materials with Schubmodule of 40 GPa | Typical for Wrought Copper Brass |
Streckgrenze Rp0,5 | 23.0 °C | 150 MPa Show Material materials with Streckgrenze Rp0,5 of 150 MPa | |
Zugfestigkeit | 23.0 °C | 380 MPa Show Material materials with Zugfestigkeit of 380 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.7E-5 - 2.1E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 - 2.1E-5 1/K | Typical for Wrought Copper Brass |
Schmelzpunkt | 875 - 1075 °C Show Material materials with Schmelzpunkt of 875 - 1075 °C | Typical for Wrought Copper Brass | |
Spezifische Wärmekapazität | 23.0 °C | 371 - 418 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Wärmeleitfähigkeit | 23.0 °C | 100 - 234 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 100 - 234 W/(m·K) | Typical for Wrought Copper Brass |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.25 % Show Material materials with Aluminium of 0.25 % |
Blei | 0.2 % Show Material materials with Blei of 0.2 % |
Eisen | 0.8 - 2 % Show Material materials with Eisen of 0.8 - 2 % |
Kupfer | 57 - 60 % Show Material materials with Kupfer of 57 - 60 % |
Mangan | 0.05 - 0.5 % Show Material materials with Mangan of 0.05 - 0.5 % |
Zinn | 0.5 - 1.5 % Show Material materials with Zinn of 0.5 - 1.5 % |