Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung A50 | 20.0 °C | 40 % Show Material materials with Dehnung A50 of 40 % |
Hardness, Rockwell F | 20.0 °C | 37 [-] Show Material materials with Hardness, Rockwell F of 37 [-] |
Streckgrenze Rp0,5 | 20.0 °C | 75 MPa Show Material materials with Streckgrenze Rp0,5 of 75 MPa |
Zugfestigkeit | 20.0 °C | 230 MPa Show Material materials with Zugfestigkeit of 230 MPa |
Chemical properties
Property | Value |
---|---|
Kupfer | 99.9 % Show Material materials with Kupfer of 99.9 % |