Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.9 g/cm³ Show Material materials with Dichte of 8.9 g/cm³ | Typical for Wrought Copper Pure / Low Alloyed Copper |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 5 % Show Material materials with Dehnung of 5 % | |
Elastizitätsmodul | 23.0 °C | 95 - 98 GPa Show Material materials with Elastizitätsmodul of 95 - 98 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Poissonzahl | 23.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Wrought Copper Pure / Low Alloyed Copper |
Schubmodule | 23.0 °C | 48 GPa Show Material materials with Schubmodule of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Streckgrenze Rp 0,2 | 23.0 °C | 385 MPa Show Material materials with Streckgrenze Rp 0,2 of 385 MPa | |
Zugfestigkeit | 23.0 °C | 435 - 495 MPa Show Material materials with Zugfestigkeit of 435 - 495 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper Pure / Low Alloyed Copper |
Schmelzpunkt | 965 - 1100 °C Show Material materials with Schmelzpunkt of 965 - 1100 °C | Typical for Wrought Copper Pure / Low Alloyed Copper | |
Spezifische Wärmekapazität | 23.0 °C | 377 - 420 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 377 - 420 J/(kg·K) | Typical for Wrought Copper Pure / Low Alloyed Copper |
Chemical properties
Property | Value |
---|---|
Kupfer | 99.75 % Show Material materials with Kupfer of 99.75 % |
Magnesium | 0.08 - 0.13 % Show Material materials with Magnesium of 0.08 - 0.13 % |
Phosphor | 0.04 - 0.08 % Show Material materials with Phosphor of 0.04 - 0.08 % |
Silber | 0.03 - 0.1 % Show Material materials with Silber of 0.03 - 0.1 % |