Mechanisch
Chemical properties
Property | Value |
---|---|
Chrom | 16 - 18 % Show Material materials with Chrom of 16 - 18 % |
Eisen | 77.83 - 83.4 % Show Material materials with Eisen of 77.83 - 83.4 % |
Kohlenstoff | 0.6 - 0.75 % Show Material materials with Kohlenstoff of 0.6 - 0.75 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 0.75 % Show Material materials with Molybdän of 0.75 % |
Nickel | 0.6 % Show Material materials with Nickel of 0.6 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Technological properties
Property | ||
---|---|---|
Processing history | cold-rolled, annealed, quenched and tempered |