Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 15 - 17 % Show Material materials with Dehnung of 15 - 17 % |
Härte, Brinell | 20.0 °C | 201 - 255 [-] Show Material materials with Härte, Brinell of 201 - 255 [-] |
Streckgrenze | 20.0 °C | 495 - 525 MPa Show Material materials with Streckgrenze of 495 - 525 MPa |
Streckgrenze Rp 0,2 | 20.0 °C | 480 - 510 MPa Show Material materials with Streckgrenze Rp 0,2 of 480 - 510 MPa |
Zugfestigkeit | 20.0 °C | 700 - 850 MPa Show Material materials with Zugfestigkeit of 700 - 850 MPa |
Chemical properties
Property | Value |
---|---|
Eisen | Balance |
Kohlenstoff | 0.32 - 0.4 % Show Material materials with Kohlenstoff of 0.32 - 0.4 % |
Mangan | 1.3 - 1.7 % Show Material materials with Mangan of 1.3 - 1.7 % |
Molybdän | 0.22 - 0.32 % Show Material materials with Molybdän of 0.22 - 0.32 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.04 % Show Material materials with Schwefel of 0.04 % |
Silizium | 0.1 - 0.4 % Show Material materials with Silizium of 0.1 - 0.4 % |