Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Medium Carbon Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 10 % Show Material materials with Dehnung of 10 % | |
Elastizitätsmodul | 20.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Medium Carbon Steel |
Härte, HBW | 20.0 °C | 207 - 225 [-] Show Material materials with Härte, HBW of 207 - 225 [-] | |
Poissonzahl | 20.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Medium Carbon Steel |
Schubmodule | 20.0 °C | 75 - 80 GPa Show Material materials with Schubmodule of 75 - 80 GPa | Typical for Carbon Steel |
Streckgrenze | 20.0 °C | 485 MPa Show Material materials with Streckgrenze of 485 MPa | |
Zugfestigkeit | 20.0 °C | 690 MPa Show Material materials with Zugfestigkeit of 690 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20.0 °C | 1.32E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32E-5 1/K | Typical for Medium Carbon Steel |
Max. Betriebstemperatur | 500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel | |
Schmelzpunkt | 1380 - 1514 °C Show Material materials with Schmelzpunkt of 1380 - 1514 °C | Typical for Medium Carbon Steel |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 20.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with spezifischer Widerstand of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Chemical properties
Property | Value | Comment |
---|---|---|
Eisen | 97.69 - 99.1 % Show Material materials with Eisen of 97.69 - 99.1 % | balance |
Kohlenstoff | 0.4 - 0.5 % Show Material materials with Kohlenstoff of 0.4 - 0.5 % | |
Mangan | 0.5 - 0.9 % Show Material materials with Mangan of 0.5 - 0.9 % | |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % | |
Schwefel | 0.045 % Show Material materials with Schwefel of 0.045 % | |
Silizium | 0.8 % Show Material materials with Silizium of 0.8 % |