Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung, transversal | 20.0 °C | 19 % Show Material materials with Dehnung, transversal of 19 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 20.0 °C | 385 MPa Show Material materials with Streckgrenze of 385 MPa | |
Streckgrenze, transversal | 20.0 °C | 385 MPa Show Material materials with Streckgrenze, transversal of 385 MPa | |
Zugfestigkeit | 20.0 °C | 530 - 680 MPa Show Material materials with Zugfestigkeit of 530 - 680 MPa | |
Zugfestigkeit, transversal | 20.0 °C | 530 - 680 MPa Show Material materials with Zugfestigkeit, transversal of 530 - 680 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % |
Kohlenstoff | 0.23 % Show Material materials with Kohlenstoff of 0.23 % |
Mangan | 1 - 1.5 % Show Material materials with Mangan of 1 - 1.5 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.035 % Show Material materials with Schwefel of 0.035 % |
Silizium | 0.55 % Show Material materials with Silizium of 0.55 % |