Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung, transversal | 20.0 °C | 18 % Show Material materials with Dehnung, transversal of 18 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 20.0 °C | 480 MPa Show Material materials with Streckgrenze of 480 MPa | |
Streckgrenze, transversal | 20.0 °C | 480 MPa Show Material materials with Streckgrenze, transversal of 480 MPa | |
Zugfestigkeit | 20.0 °C | 600 - 750 MPa Show Material materials with Zugfestigkeit of 600 - 750 MPa | |
Zugfestigkeit, transversal | 20.0 °C | 600 - 750 MPa Show Material materials with Zugfestigkeit, transversal of 600 - 750 MPa |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 0.16 % Show Material materials with Kohlenstoff of 0.16 % |
Mangan | 1.1 - 1.7 % Show Material materials with Mangan of 1.1 - 1.7 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.25 % Show Material materials with Schwefel of 0.25 % |
Silizium | 0.55 % Show Material materials with Silizium of 0.55 % |