Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Chromium Molybdenum Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Chromium Molybdenum Steel |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Chromium Molybdenum Steel |
Streckgrenze Rp 0,2 | 100.0 °C | 338 MPa Show Material materials with Streckgrenze Rp 0,2 of 338 MPa | |
150.0 °C | 319 MPa Show Material materials with Streckgrenze Rp 0,2 of 319 MPa | ||
200.0 °C | 319 MPa Show Material materials with Streckgrenze Rp 0,2 of 319 MPa | ||
250.0 °C | 309 MPa Show Material materials with Streckgrenze Rp 0,2 of 309 MPa | ||
300.0 °C | 304 MPa Show Material materials with Streckgrenze Rp 0,2 of 304 MPa | ||
350.0 °C | 294 MPa Show Material materials with Streckgrenze Rp 0,2 of 294 MPa | ||
400.0 °C | 284 MPa Show Material materials with Streckgrenze Rp 0,2 of 284 MPa | ||
450.0 °C | 275 MPa Show Material materials with Streckgrenze Rp 0,2 of 275 MPa | ||
Zugfestigkeit | 100.0 °C | 500 MPa Show Material materials with Zugfestigkeit of 500 MPa | |
150.0 °C | 480 MPa Show Material materials with Zugfestigkeit of 480 MPa | ||
200.0 °C | 460 MPa Show Material materials with Zugfestigkeit of 460 MPa | ||
250.0 °C | 450 MPa Show Material materials with Zugfestigkeit of 450 MPa | ||
300.0 °C | 440 MPa Show Material materials with Zugfestigkeit of 440 MPa | ||
350.0 °C | 430 MPa Show Material materials with Zugfestigkeit of 430 MPa | ||
400.0 °C | 410 MPa Show Material materials with Zugfestigkeit of 410 MPa | ||
450.0 °C | 380 MPa Show Material materials with Zugfestigkeit of 380 MPa | ||
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.1E-5 - 1.4E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.1E-5 - 1.4E-5 1/K | Typical for Chromium Molybdenum Steel |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Chromium Molybdenum Steel | |
Spezifische Wärmekapazität | 23.0 °C | 448 - 502 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 448 - 502 J/(kg·K) | Typical for Chromium Molybdenum Steel |
Wärmeleitfähigkeit | 23.0 °C | 36 - 43 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 36 - 43 W/(m·K) | Typical for Chromium Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 2.65 - 3.35 % Show Material materials with Chrom of 2.65 - 3.35 % |
Kohlenstoff | 0.06 - 0.15 % Show Material materials with Kohlenstoff of 0.06 - 0.15 % |
Mangan | 0.3 - 0.6 % Show Material materials with Mangan of 0.3 - 0.6 % |
Molybdän | 0.8 - 1.06 % Show Material materials with Molybdän of 0.8 - 1.06 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |