Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ | Typical for Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 14 % Show Material materials with Dehnung of 14 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 20.0 °C | 690 MPa Show Material materials with Streckgrenze of 690 MPa | |
Zugfestigkeit | 20.0 °C | 790 - 940 MPa Show Material materials with Zugfestigkeit of 790 - 940 MPa |
Thermisch
Property | Value |
---|---|
Max. Betriebstemperatur, lang | -60 - 0 °C Show Material materials with Max. Betriebstemperatur, lang of -60 - 0 °C |
Chemical properties
Property | Value |
---|---|
Chrom | 0.5 - 1 % Show Material materials with Chrom of 0.5 - 1 % |
Kohlenstoff | 0.2 % Show Material materials with Kohlenstoff of 0.2 % |
Mangan | 0.7 - 1.2 % Show Material materials with Mangan of 0.7 - 1.2 % |
Molybdän | 0.2 - 0.6 % Show Material materials with Molybdän of 0.2 - 0.6 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Silizium | 0.4 - 0.8 % Show Material materials with Silizium of 0.4 - 0.8 % |
Zirkonium | 0.12 % Show Material materials with Zirkonium of 0.12 % |