Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.9 g/cm³ Show Material materials with Dichte of 7.9 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 20 % Show Material materials with Dehnung of 20 % |
Streckgrenze Rp 0,2 | 20.0 °C | 315 MPa Show Material materials with Streckgrenze Rp 0,2 of 315 MPa |
100.0 °C | 220 MPa Show Material materials with Streckgrenze Rp 0,2 of 220 MPa | |
200.0 °C | 170 MPa Show Material materials with Streckgrenze Rp 0,2 of 170 MPa | |
300.0 °C | 140 MPa Show Material materials with Streckgrenze Rp 0,2 of 140 MPa | |
350.0 °C | 130 MPa Show Material materials with Streckgrenze Rp 0,2 of 130 MPa | |
400.0 °C | 120 MPa Show Material materials with Streckgrenze Rp 0,2 of 120 MPa | |
Streckgrenze Rp 1,0 | 20.0 °C | 340 MPa Show Material materials with Streckgrenze Rp 1,0 of 340 MPa |
Zugfestigkeit | 20.0 °C | 570 - 800 MPa Show Material materials with Zugfestigkeit of 570 - 800 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 1.57E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.57E-5 1/K |
200.0 °C | 1.7E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 1/K | |
300.0 °C | 1.75E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.75E-5 1/K | |
Spezifische Wärmekapazität | 20.0 °C | 500 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 500 J/(kg·K) |
Wärmeleitfähigkeit | 20.0 °C | 14 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 14 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Chrom | 20 - 22 % Show Material materials with Chrom of 20 - 22 % |
Kohlenstoff | 0.03 % Show Material materials with Kohlenstoff of 0.03 % |
Mangan | 3 - 6 % Show Material materials with Mangan of 3 - 6 % |
Molybdän | 3 - 3.5 % Show Material materials with Molybdän of 3 - 3.5 % |
Nickel | 14 - 17 % Show Material materials with Nickel of 14 - 17 % |
Niobium | 0.25 % Show Material materials with Niobium of 0.25 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Stickstoff | 0.2 - 0.35 % Show Material materials with Stickstoff of 0.2 - 0.35 % |