Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.9 g/cm³ Show Material materials with Dichte of 7.9 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 30 % Show Material materials with Dehnung of 30 % | |
Elastizitätsmodul | 23.0 °C | 195 GPa Show Material materials with Elastizitätsmodul of 195 GPa | Typical for Austenitic Stainless Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Austenitic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Austenitic Stainless Steel |
Streckgrenze Rp 0,2 | 20.0 °C | 205 MPa Show Material materials with Streckgrenze Rp 0,2 of 205 MPa | |
100.0 °C | 140 MPa Show Material materials with Streckgrenze Rp 0,2 of 140 MPa | ||
200.0 °C | 110 MPa Show Material materials with Streckgrenze Rp 0,2 of 110 MPa | ||
300.0 °C | 92 MPa Show Material materials with Streckgrenze Rp 0,2 of 92 MPa | ||
350.0 °C | 85 MPa Show Material materials with Streckgrenze Rp 0,2 of 85 MPa | ||
400.0 °C | 80 MPa Show Material materials with Streckgrenze Rp 0,2 of 80 MPa | ||
Streckgrenze Rp 1,0 | 20.0 °C | 230 MPa Show Material materials with Streckgrenze Rp 1,0 of 230 MPa | |
Zugfestigkeit | 20.0 °C | 440 - 640 MPa Show Material materials with Zugfestigkeit of 440 - 640 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 1.65E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.65E-5 1/K | |
200.0 °C | 1.75E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.75E-5 1/K | ||
300.0 °C | 1.75E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.75E-5 1/K | ||
400.0 °C | 1.85E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.85E-5 1/K | ||
Schmelzpunkt | 1230 - 1480 °C Show Material materials with Schmelzpunkt of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Spezifische Wärmekapazität | 20.0 °C | 500 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 500 J/(kg·K) | |
Wärmeleitfähigkeit | 20.0 °C | 15 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 15 W/(m·K) |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 8.5E-7 Ω·m Show Material materials with spezifischer Widerstand of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 17 - 20 % Show Material materials with Chrom of 17 - 20 % |
Kohlenstoff | 0.03 % Show Material materials with Kohlenstoff of 0.03 % |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % |
Molybdän | 2 - 3 % Show Material materials with Molybdän of 2 - 3 % |
Nickel | 9 - 13 % Show Material materials with Nickel of 9 - 13 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % |
Silizium | 1.5 % Show Material materials with Silizium of 1.5 % |
Stickstoff | 0.1 - 0.2 % Show Material materials with Stickstoff of 0.1 - 0.2 % |