Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 22 % Show Material materials with Dehnung of 22 % | |
Elastizitätsmodul | 23.0 °C | 200 GPa Show Material materials with Elastizitätsmodul of 200 GPa | Typical for Duplex Stainless Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Duplex Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Duplex Stainless Steel |
Streckgrenze Rp 0,2 | 20.0 °C | 480 MPa Show Material materials with Streckgrenze Rp 0,2 of 480 MPa | |
100.0 °C | 390 MPa Show Material materials with Streckgrenze Rp 0,2 of 390 MPa | ||
200.0 °C | 330 MPa Show Material materials with Streckgrenze Rp 0,2 of 330 MPa | ||
300.0 °C | 295 MPa Show Material materials with Streckgrenze Rp 0,2 of 295 MPa | ||
350.0 °C | 280 MPa Show Material materials with Streckgrenze Rp 0,2 of 280 MPa | ||
Zugfestigkeit | 20.0 °C | 650 - 850 MPa Show Material materials with Zugfestigkeit of 650 - 850 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 1.4E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.4E-5 1/K | |
200.0 °C | 1.45E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.45E-5 1/K | ||
300.0 °C | 1.49E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.49E-5 1/K | ||
Max. Betriebstemperatur | 300 °C Show Material materials with Max. Betriebstemperatur of 300 °C | Typical for Duplex Stainless Steel | |
Max. Betriebstemperatur, lang | 0 - 300 °C Show Material materials with Max. Betriebstemperatur, lang of 0 - 300 °C | ||
Schmelzpunkt | 1375 - 1450 °C Show Material materials with Schmelzpunkt of 1375 - 1450 °C | Typical for Duplex Stainless Steel | |
Spezifische Wärmekapazität | 20.0 °C | 450 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 450 J/(kg·K) | |
Wärmeleitfähigkeit | 20.0 °C | 15 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 15 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Chrom | 24 - 26 % Show Material materials with Chrom of 24 - 26 % |
Kohlenstoff | 0.03 % Show Material materials with Kohlenstoff of 0.03 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Molybdän | 4 - 5 % Show Material materials with Molybdän of 4 - 5 % |
Nickel | 6 - 8 % Show Material materials with Nickel of 6 - 8 % |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % |
Silizium | 1 % Show Material materials with Silizium of 1 % |
Stickstoff | 0.12 - 0.25 % Show Material materials with Stickstoff of 0.12 - 0.25 % |