Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.7 g/cm³ Show Material materials with Dichte of 7.7 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 220 GPa Show Material materials with Elastizitätsmodul of 220 GPa | Typical for Martensitic Stainless Steel |
Härte, Brinell | 20.0 °C | 350 [-] Show Material materials with Härte, Brinell of 350 [-] | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Martensitic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Martensitic Stainless Steel |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 400.0 °C | 1.25E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.25E-5 1/K | |
800.0 °C | 1.35E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.35E-5 1/K | ||
Max. Betriebstemperatur, lang | 0 - 900 °C Show Material materials with Max. Betriebstemperatur, lang of 0 - 900 °C | ||
Schmelzpunkt | 1370 - 1530 °C Show Material materials with Schmelzpunkt of 1370 - 1530 °C | Typical for Martensitic Stainless Steel | |
Spezifische Wärmekapazität | 20.0 °C | 500 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 500 J/(kg·K) | |
Wärmeleitfähigkeit | 20.0 °C | 18.8 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 18.8 W/(m·K) |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 6E-7 Ω·m Show Material materials with spezifischer Widerstand of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 17 - 19 % Show Material materials with Chrom of 17 - 19 % |
Kohlenstoff | 1.4 - 1.8 % Show Material materials with Kohlenstoff of 1.4 - 1.8 % |
Mangan | 0.5 - 1 % Show Material materials with Mangan of 0.5 - 1 % |
Phosphor | 0.05 % Show Material materials with Phosphor of 0.05 % |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % |
Silizium | 1 - 2.5 % Show Material materials with Silizium of 1 - 2.5 % |