Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Nickel Molybdenum Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 16 % Show Material materials with Dehnung of 16 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Nickel Molybdenum Steel |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Nickel Molybdenum Steel |
Streckgrenze | 20.0 °C | 400 - 450 MPa Show Material materials with Streckgrenze of 400 - 450 MPa | |
Zugfestigkeit | 20.0 °C | 550 - 750 MPa Show Material materials with Zugfestigkeit of 550 - 750 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 9E-6 - 1.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9E-6 - 1.3E-5 1/K | Typical for Nickel Molybdenum Steel |
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Nickel Molybdenum Steel | |
Spezifische Wärmekapazität | 23.0 °C | 335 - 481 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 335 - 481 J/(kg·K) | Typical for Nickel Molybdenum Steel |
Wärmeleitfähigkeit | 23.0 °C | 44 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 44 W/(m·K) | Typical for Nickel Molybdenum Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 0.3 % Show Material materials with Chrom of 0.3 % |
Kohlenstoff | 0.17 - 0.23 % Show Material materials with Kohlenstoff of 0.17 - 0.23 % |
Mangan | 1.2 - 1.5 % Show Material materials with Mangan of 1.2 - 1.5 % |
Molybdän | 0.45 - 0.6 % Show Material materials with Molybdän of 0.45 - 0.6 % |
Nickel | 0.5 - 0.8 % Show Material materials with Nickel of 0.5 - 0.8 % |
Phosphor | 0.02 % Show Material materials with Phosphor of 0.02 % |
Schwefel | 0.015 % Show Material materials with Schwefel of 0.015 % |
Silizium | 0.6 % Show Material materials with Silizium of 0.6 % |