Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Nickel Chromium Molybdenum Steel |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 16 % Show Material materials with Dehnung of 16 % | |
Elastizitätsmodul | 23.0 °C | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Nickel Chromium Molybdenum Steel |
Poissonzahl | 23.0 °C | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Nickel Chromium Molybdenum Steel |
Streckgrenze | 20.0 °C | 550 MPa Show Material materials with Streckgrenze of 550 MPa | |
Zugfestigkeit | 20.0 °C | 650 - 800 MPa Show Material materials with Zugfestigkeit of 650 - 800 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | -196.0 °C | 8.6E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8.6E-6 1/K | |
-170.0 °C | 9.4E-6 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9.4E-6 1/K | ||
-120.0 °C | 1.03E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.03E-5 1/K | ||
-50.0 °C | 1.12E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.12E-5 1/K | ||
-25.0 °C | 1.14E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.14E-5 1/K | ||
Schmelzpunkt | 1382 - 1529 °C Show Material materials with Schmelzpunkt of 1382 - 1529 °C | Typical for Nickel Chromium Molybdenum Steel | |
Spezifische Wärmekapazität | 23.0 °C | 448 - 670 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 448 - 670 J/(kg·K) | Typical for Nickel Chromium Molybdenum Steel |
Wärmeleitfähigkeit | -20.0 °C | 35 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 35 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Chrom | 1.3 - 1.8 % Show Material materials with Chrom of 1.3 - 1.8 % |
Kohlenstoff | 0.12 - 0.16 % Show Material materials with Kohlenstoff of 0.12 - 0.16 % |
Mangan | 0.55 - 0.7 % Show Material materials with Mangan of 0.55 - 0.7 % |
Molybdän | 0.45 - 0.55 % Show Material materials with Molybdän of 0.45 - 0.55 % |
Nickel | 2.7 - 3 % Show Material materials with Nickel of 2.7 - 3 % |
Phosphor | 0.01 % Show Material materials with Phosphor of 0.01 % |
Schwefel | 0.01 % Show Material materials with Schwefel of 0.01 % |
Silizium | 0.3 % Show Material materials with Silizium of 0.3 % |