Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.85 g/cm³ Show Material materials with Dichte of 7.85 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung, transversal | 20.0 °C | 12 - 13 % Show Material materials with Dehnung, transversal of 12 - 13 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Flächenreduzierung, transversal | 20.0 °C | 40 % Show Material materials with Flächenreduzierung, transversal of 40 % | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze Rp 0,2 | 100.0 °C | 585 MPa Show Material materials with Streckgrenze Rp 0,2 of 585 MPa | |
200.0 °C | 560 MPa Show Material materials with Streckgrenze Rp 0,2 of 560 MPa | ||
250.0 °C | 550 MPa Show Material materials with Streckgrenze Rp 0,2 of 550 MPa | ||
300.0 °C | 535 MPa Show Material materials with Streckgrenze Rp 0,2 of 535 MPa | ||
350.0 °C | 520 MPa Show Material materials with Streckgrenze Rp 0,2 of 520 MPa | ||
400.0 °C | 500 MPa Show Material materials with Streckgrenze Rp 0,2 of 500 MPa | ||
450.0 °C | 480 MPa Show Material materials with Streckgrenze Rp 0,2 of 480 MPa | ||
500.0 °C | 440 MPa Show Material materials with Streckgrenze Rp 0,2 of 440 MPa | ||
Streckgrenze Rp 0,2, transversal | 20.0 °C | 560 - 700 MPa Show Material materials with Streckgrenze Rp 0,2, transversal of 560 - 700 MPa | |
Zugfestigkeit, transversal | 20.0 °C | 650 - 930 MPa Show Material materials with Zugfestigkeit, transversal of 650 - 930 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Chrom | 2 - 2.2 % Show Material materials with Chrom of 2 - 2.2 % |
Kohlenstoff | 0.2 - 0.24 % Show Material materials with Kohlenstoff of 0.2 - 0.24 % |
Mangan | 0.6 - 0.8 % Show Material materials with Mangan of 0.6 - 0.8 % |
Molybdän | 0.8 - 0.9 % Show Material materials with Molybdän of 0.8 - 0.9 % |
Nickel | 0.7 - 0.8 % Show Material materials with Nickel of 0.7 - 0.8 % |
Phosphor | 0.01 % Show Material materials with Phosphor of 0.01 % |
Schwefel | 7E-3 % Show Material materials with Schwefel of 7E-3 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Vanadium | 0.25 - 0.35 % Show Material materials with Vanadium of 0.25 - 0.35 % |
Wolfram | 0.6 - 0.7 % Show Material materials with Wolfram of 0.6 - 0.7 % |