Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.85 g/cm³ Show Material materials with Dichte of 7.85 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 11 % Show Material materials with Dehnung of 11 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 20.0 °C | 520 MPa Show Material materials with Streckgrenze of 520 MPa | |
Zugfestigkeit | 20.0 °C | 736 MPa Show Material materials with Zugfestigkeit of 736 MPa |
Chemical properties
Property | Value |
---|---|
Chrom | 0.9 - 1.2 % Show Material materials with Chrom of 0.9 - 1.2 % |
Kohlenstoff | 0.46 - 0.54 % Show Material materials with Kohlenstoff of 0.46 - 0.54 % |
Mangan | 0.5 - 0.8 % Show Material materials with Mangan of 0.5 - 0.8 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.035 % Show Material materials with Schwefel of 0.035 % |
Silizium | 0.25 - 0.5 % Show Material materials with Silizium of 0.25 - 0.5 % |
Vanadium | 0.07 - 0.12 % Show Material materials with Vanadium of 0.07 - 0.12 % |