Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.85 g/cm³ Show Material materials with Dichte of 7.85 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 14 % Show Material materials with Dehnung of 14 % | |
Elastizitätsmodul | 23.0 °C | 190 - 210 GPa Show Material materials with Elastizitätsmodul of 190 - 210 GPa | Typical for Steel |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 20.0 °C | 334 MPa Show Material materials with Streckgrenze of 334 MPa | |
Zugfestigkeit | 20.0 °C | 589 MPa Show Material materials with Zugfestigkeit of 589 MPa |
Chemical properties
Property | Value |
---|---|
Kohlenstoff | 0.42 - 0.5 % Show Material materials with Kohlenstoff of 0.42 - 0.5 % |
Mangan | 0.9 - 1.2 % Show Material materials with Mangan of 0.9 - 1.2 % |
Phosphor | 0.04 % Show Material materials with Phosphor of 0.04 % |
Schwefel | 0.035 % Show Material materials with Schwefel of 0.035 % |
Silizium | 0.25 - 0.5 % Show Material materials with Silizium of 0.25 - 0.5 % |