Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 18.3 % Show Material materials with Dehnung of 18.3 % | Predicted Value, A200 | ||||
21.0 % Show Material materials with Dehnung of 21.0 % | Predicted Value, A80 Transverse | |||||
21.3 % Show Material materials with Dehnung of 21.3 % | Predicted Value, A5 | |||||
22.2 % Show Material materials with Dehnung of 22.2 % | Predicted Value, A50 | |||||
23.1 % Show Material materials with Dehnung of 23.1 % | Predicted Value, Transverse | |||||
20 °C | 20 % Show Material materials with Dehnung of 20 % | thermomechanically rolled | EN 10149-2 | Flat | A80 | |
20 °C | 24 % Show Material materials with Dehnung of 24 % | thermomechanically rolled | EN 10149-2 | Flat | ||
Elastizitätsmodul | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Low Carbon Steel | ||||
Flächenreduzierung | 40.6 % Show Material materials with Flächenreduzierung of 40.6 % | Predicted Value | ||||
44.4 % Show Material materials with Flächenreduzierung of 44.4 % | Predicted Value, Transverse | |||||
Härte, Brinell | 241 [-] Show Material materials with Härte, Brinell of 241 [-] | Predicted Value, Transverse | ||||
Poissonzahl | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Low Carbon Steel | ||||
Scherfestigkeit | 532.2 MPa Show Material materials with Scherfestigkeit of 532.2 MPa | Predicted Value | ||||
Schubmodule | 82 GPa Show Material materials with Schubmodule of 82 GPa | Typical for Low Carbon Steel | ||||
Streckgrenze | 251.8 MPa Show Material materials with Streckgrenze of 251.8 MPa | Predicted Value, RP1 | ||||
315.4 MPa Show Material materials with Streckgrenze of 315.4 MPa | Predicted Value, RP1 Transverse | |||||
332.9 MPa Show Material materials with Streckgrenze of 332.9 MPa | Predicted Value, RP02 | |||||
345.1 MPa Show Material materials with Streckgrenze of 345.1 MPa | Predicted Value, Transverse | |||||
405.9 MPa Show Material materials with Streckgrenze of 405.9 MPa | Predicted Value, RP05 | |||||
483.3 MPa Show Material materials with Streckgrenze of 483.3 MPa | Predicted Value, RP02 Transverse | |||||
488 MPa Show Material materials with Streckgrenze of 488 MPa | Predicted Value, RP002 | |||||
20 °C | 315 MPa Show Material materials with Streckgrenze of 315 MPa | thermomechanically rolled | EN 10149-2 | Flat | ||
Zugfestigkeit | 20 °C | 390 - 510 MPa Show Material materials with Zugfestigkeit of 390 - 510 MPa | thermomechanically rolled | EN 10149-2 | Flat |
Thermisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 1.32e-05 - 1.38e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel | |||
Max. Betriebstemperatur | -20 °C Show Material materials with Max. Betriebstemperatur of -20 °C | thermomechanically rolled | EN 10149-2 | Flat | Long |
500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel | ||||
Schmelzpunkt | 1480 - 1526 °C Show Material materials with Schmelzpunkt of 1480 - 1526 °C | Typical for Low Carbon Steel | |||
Spezifische Wärmekapazität | 465 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 465 J/(kg·K) | Typical for Low Carbon Steel | |||
Wärmeleitfähigkeit | 25 - 93 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 7 S/m Show Material materials with Elektrische Leitfähigkeit of 7 S/m | Predicted Value |
spezifischer Widerstand | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with spezifischer Widerstand of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnetisch
Property | Value | Comment |
---|---|---|
Curie-Temperatur | 770 °C Show Material materials with Curie-Temperatur of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 0.015 % Show Material materials with Aluminium of 0.015 % | thermomechanically rolled | EN 10149-2 | Flat |
Kohlenstoff | 0.12 % Show Material materials with Kohlenstoff of 0.12 % | thermomechanically rolled | EN 10149-2 | Flat |
Mangan | 1.3 % Show Material materials with Mangan of 1.3 % | thermomechanically rolled | EN 10149-2 | Flat |
Niobium | 0.09 % Show Material materials with Niobium of 0.09 % | thermomechanically rolled | EN 10149-2 | Flat |
Phosphor | 0.025 % Show Material materials with Phosphor of 0.025 % | thermomechanically rolled | EN 10149-2 | Flat |
Schwefel | 0.02 % Show Material materials with Schwefel of 0.02 % | thermomechanically rolled | EN 10149-2 | Flat |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % | thermomechanically rolled | EN 10149-2 | Flat |
Titan | 0.15 % Show Material materials with Titan of 0.15 % | thermomechanically rolled | EN 10149-2 | Flat |
Vanadium | 0.2 % Show Material materials with Vanadium of 0.2 % | thermomechanically rolled | EN 10149-2 | Flat |