Allgemein
Property | Value | Comment |
---|---|---|
Dichte | 7.8 - 7.9 g/cm³ Show Material materials with Dichte of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 20.1 % Show Material materials with Dehnung of 20.1 % | Predicted Value, Transverse | ||||
20.4 % Show Material materials with Dehnung of 20.4 % | Predicted Value, A200 | |||||
21.5 % Show Material materials with Dehnung of 21.5 % | Predicted Value, A5 | |||||
24 % Show Material materials with Dehnung of 24 % | Predicted Value, A80 Transverse | |||||
37.0 % Show Material materials with Dehnung of 37.0 % | Predicted Value | |||||
38.0 % Show Material materials with Dehnung of 38.0 % | Predicted Value, A50 | |||||
20 °C | 38 % Show Material materials with Dehnung of 38 % | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | A80 | |
Elastizitätsmodul | 200 - 215 GPa Show Material materials with Elastizitätsmodul of 200 - 215 GPa | Typical for Low Carbon Steel | ||||
Flächenreduzierung | 43.1 % Show Material materials with Flächenreduzierung of 43.1 % | Predicted Value, Transverse | ||||
45.5 % Show Material materials with Flächenreduzierung of 45.5 % | Predicted Value | |||||
Härte, Brinell | 266 [-] Show Material materials with Härte, Brinell of 266 [-] | Predicted Value, Transverse | ||||
Poissonzahl | 0.29 [-] Show Material materials with Poissonzahl of 0.29 [-] | Typical for Low Carbon Steel | ||||
Scherfestigkeit | 564 MPa Show Material materials with Scherfestigkeit of 564 MPa | Predicted Value | ||||
Schubmodule | 82 GPa Show Material materials with Schubmodule of 82 GPa | Typical for Low Carbon Steel | ||||
Streckgrenze | 256.6 MPa Show Material materials with Streckgrenze of 256.6 MPa | Predicted Value, RP1 | ||||
260.2 MPa Show Material materials with Streckgrenze of 260.2 MPa | Predicted Value, RP05 | |||||
289.9 MPa Show Material materials with Streckgrenze of 289.9 MPa | Predicted Value, Transverse | |||||
312.8 MPa Show Material materials with Streckgrenze of 312.8 MPa | Predicted Value, RP02 | |||||
315.1 MPa Show Material materials with Streckgrenze of 315.1 MPa | Predicted Value, RP1 Transverse | |||||
452.5 MPa Show Material materials with Streckgrenze of 452.5 MPa | Predicted Value, RP02 Transverse | |||||
489.2 MPa Show Material materials with Streckgrenze of 489.2 MPa | Predicted Value, RP002 | |||||
20 °C | 140 - 210 MPa Show Material materials with Streckgrenze of 140 - 210 MPa | skin passed | EN 10130 | Sheet, Flat, Bar, Strip | ||
Zugfestigkeit | 20 °C | 270 - 350 MPa Show Material materials with Zugfestigkeit of 270 - 350 MPa | skin passed | EN 10130 | Sheet, Flat, Bar, Strip |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.32e-05 - 1.38e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.32e-05 - 1.38e-05 1/K | Typical for Low Carbon Steel |
Max. Betriebstemperatur | 323.1 °C Show Material materials with Max. Betriebstemperatur of 323.1 °C | Predicted Value, Long |
500 °C Show Material materials with Max. Betriebstemperatur of 500 °C | Typical for Carbon Steel | |
Schmelzpunkt | 1480 - 1526 °C Show Material materials with Schmelzpunkt of 1480 - 1526 °C | Typical for Low Carbon Steel |
Spezifische Wärmekapazität | 465 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 465 J/(kg·K) | Typical for Low Carbon Steel |
Wärmeleitfähigkeit | 25 - 93 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Elektrisch
Property | Value | Comment |
---|---|---|
Elektrische Leitfähigkeit | 8 S/m Show Material materials with Elektrische Leitfähigkeit of 8 S/m | Predicted Value |
spezifischer Widerstand | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with spezifischer Widerstand of 1.43e-07 - 1.74e-07 Ω·m | Typical for Carbon Steel |
Magnetisch
Property | Value | Comment |
---|---|---|
Curie-Temperatur | 770 °C Show Material materials with Curie-Temperatur of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Kohlenstoff | 0.08 % Show Material materials with Kohlenstoff of 0.08 % | skin passed | EN 10130 | Sheet, Flat, Bar, Strip |
Mangan | 0.4 % Show Material materials with Mangan of 0.4 % | skin passed | EN 10130 | Sheet, Flat, Bar, Strip |
Phosphor | 0.03 % Show Material materials with Phosphor of 0.03 % | skin passed | EN 10130 | Sheet, Flat, Bar, Strip |
Schwefel | 0.03 % Show Material materials with Schwefel of 0.03 % | skin passed | EN 10130 | Sheet, Flat, Bar, Strip |